SMC
Physical Property | Units | Data | Standard |
Glass fiber content | % | 28±2 | |
Density | ( g/cm³) | 1.75-1.9 | ASTM D-792 |
Water absorption | mg | ≤20 | ASTM D-570 |
Average Shrinkage | % | ≤0.15 | ASTM D-955 |
Tensile Strength | Mpa | ≥70 | ASTM D-638 |
Flexural Strength | Mpa | ≥160 | ASTM D-790 |
Impact Strength-Izod Unnotched | kj/m2 | ≥65 | ASTM D-4812 |
Barcol Hardness | - | >50 | ASTM D-2583 |
Heat Distortion Temp | C | ≥200 | ASTM D-648 |
Color | - | 7035 etc | RAL |
Physical Property | Units | Data | Standard |
Glass fiber content | % | 31±2 | |
Density | ( g/cm³) | 1.75-1.9 | ASTM D-792 |
Water absorption | mg | ≤20 | ASTM D-570 |
Average Shrinkage | % | ≤0.15 | ASTM D-955 |
Tensile Strength | Mpa | ≥85 | ASTM D-638 |
Flexural Strength | Mpa | ≥180 | ASTM D-790 |
Impact Strength-Izod Unnotched | kj/m2 | ≥80 | ASTM D-4812 |
Barcol Hardness | - | >50 | ASTM D-2583 |
Heat Distortion Temp | ℃ | ≥200 | ASTM D-648 |
Color | - | 7035 etc | RAL |
Physical Property | Units | Data | Standard |
Glass fiber content | % | 28±2 | |
Density | ( g/cm³) | 1.75-1.9 | ASTM D-792 |
Water absorption | mg | ≤20 | ASTM D-570 |
Average Shrinkage | % | ≤0.15 | ASTM D-955 |
Tensile Strength | Mpa | ≥70 | ASTM D-638 |
Flexural Strength | Mpa | ≥160 | ASTM D-790 |
Impact Strength-Izod Unnotched | kj/m2 | ≥65 | ASTM D-4812 |
Barcol Hardness | - | >50 | ASTM D-2583 |
Heat Distortion Temp | C | ≥200 | ASTM D-648 |
Color | - | 7035 etc | RAL |